Dafnelen®
Polipropilene compound Omopolimero o Copolimero non caricato, con elevate proprietà meccaniche, sviluppato seguendo le richieste del mercato e gli standard industriali. Prodotti disponibili in un’ampia gamma di colori e in versioni autoestinguenti certificate, alogenate o esente alogeni.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Dafnelen® CR 09/K | PP copo flame retardant halogen free UL94 V0 (0,8mm) | 10 g/10' | - | 1900 MPa | - | 3,5 Kj/m2 | - | Classe V0-5VA YC | |
Dafnelen® HP 1003/S | 50% glass fibers chemical grafting. | 3 g/10' | - | 10500 Mpa | - | 12 KJ/m2 | - | Classe HB | |
Dafnelen® HP 505/SW | PP homo 25% glass fiber, flame retardant V0 | 5 g/10' | - | 6500 MPa | - | 6 Kj/m2 | - | Classe V0 | |
Dafnelen® HP 605/SW | PP homo 30% glass fiber, flame retardant V0 | 4 g/10' | - | 8000 MPa | - | 7 Kj/m2 | - | Classe V0 YC | |
Dafnelen® HR 17/Y | Unfilled homopolymer polypropylene.Flame Retardant grade Halogen-free according to IEC 61249-2-21 | 17 g/10' | - | 1500 Mpa | - | 5 KJ/m2 | - | Classe V2 |
Dafneglass®
Polipropilene compound rinforzato con fibre di vetro, legate chimicamente o meccanicamente, con elevate proprietà termiche, di resistenza all’impatto e di rigidità, in accordo con gli standard delle industrie automobilistiche e dell’elettrodomestico. Prodotti disponibili nelle colorazioni e nelle versioni autoestinguenti indicate per i relativi settori, con importanti certificazioni per alogenati e esente alogeni.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Dafneglass® HP 505/K | PP homo 25% glass fiber, flame retardant grade without halogens, heat stabilized. | 3,5 g/10' | - | 7000 MPa | - | 7,3 Kj/m2 | - | Classe V0 | |
Dafneglass® HP 605/K | 30% chemically coupled glass fiber reinforced polypropylene. V0 flame retardant grade. Heat stabilized. Flame Retardant grade Without halogens. | 2 g/10' | - | 7600 Mpa | - | 8 KJ/m2 | - | Classe HB |
Isoplen®
Polipropilene compound Omopolimero o Copolimero non caricato, con elevate proprietà meccaniche, sviluppato seguendo le richieste del mercato e gli standard industriali. Prodotti disponibili in un’ampia gamma di colori e in versioni autoestinguenti certificate, alogenate o esente alogeni.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Isoplen® A H F | PP homo, natural colour medium flowability | 12 g/10' | - | 1400 MPa | - | 3,3 Kj/m2 | - | Classe HB | |
Isoplen® A K F | PP copo, medium flowability | 13 g/10' | - | 1300 MPa | - | 11 Kj/m2 | - | Classe HB | |
Isoplen® A K Z | PP copo, high flowability | 21 g/10' | - | 1350 MPa | - | 5,6 Kj/m2 | - | Classe HB | |
Isoplen® FR V2 | PP copo flame retardant low halogen content | 10 g/10' | - | 1400 MPa | - | 10 Kj/m2 | - | Classe V2 YC | |
Isoplen® H2 T V | PP homo, natural colour, heat stabilized, high flowability | 20 g/10' | - | 1400 MPa | - | 5 Kj/m2 | - | Classe HB | |
Isoplen® HK X V0 HF | Unfilled. Heat stabilized. Flame Retardant grade without halogens. | 10 g/10' | - | 1600 Mpa | - | 3,5 KJ/m2 | - | Classe V0 YC |
Isoflex®
Polipropilene copolimero, non caricato e non stabilizzatoNome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Isoflex® C800 | Polypropylene copolymer. | 6 g/10' | - | 800 Mpa | - | 45 KJ/m2 | - | / |
Isofil®
Polipropilene compound additivato con cariche minerali (T/TC/CaCO3/BaSO4/Mica) standard o ad alte prestazioni, in accordo con le richieste del mercato e gli standard industriali. Prodotti sviluppati per soddisfare il cliente a seconda delle diverse applicazioni, in termini di colori e specifiche tecniche. Disponibili versioni autoestinguenti certificate, alogenate o esente alogeni.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Isofil® H 20 T F UV | 20% talc filled homopolymer polypropylene. UV stabilized. | 15 g/10' | - | 2600 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® H 20 TP F HS | 20% Talc filled polypropylene homopolymer. Low emission. Compliant to VW44045-PP6.Heat stabilized. | 12 g/10' | - | 2800 Mpa | - | 3 KJ/m2 | - | Classe Hb | |
Isofil® H 20 TP X | PP homo 20% talc natural colour | 9 g/10' | - | 2600 MPa | - | 3 Kj/m2 | - | Classe HB | |
Isofil® H 40 C2 F | 40% calcium carbonate filled homopolymer polypropylene. | 13 g/10' | - | 2500 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® H 40 C2 X | 40% calcite filled homopolymer polypropylene. | 9 g/10' | - | 2400 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® H 40 TG S HS | 40% talc filled polypropylene homopolymer. | 10 kg/10' | - | 4100 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® H 40 TG X HS | 40% talc filled homopolymer polypropylene. Compliant to VW 44045-PP8. Heat stabilized. | 15 g/10' | - | 4000 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® H 40 TP F | PP homo 40% talc | 12 g/10' | - | 4000 MPa | - | 2,4 Kj/m2 | - | Classe HB | |
Isofil® HF 2206H L | 10% talc filled polypropylene copolymer. Heat stabilized. Laserable. | 12 g/10' | - | 1500 Mpa | - | 8 KJ/m2 | - | Classe HB | |
Isofil® HF 6205X | 30% talc filled copolymer polypropylene. UV stabilized. Heat stabilized. | 14 g/10' | - | 2300 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isofil® HK 10 TVHM | 10% micro talc filled polypropylene. White colour. | 20 g/10' | - | 2400 MPa | - | 4 Kj/m2 | - | Classe HB YC | |
Isofil® HK 20 2VH0 | 20% calcium carbonate polypropylene. Heat stabilized. | 16 g/10' | - | 1850 Mpa | - | 2,4 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 T V0 | 20% talc filled copolymer polypropylene. Heat stabilized. Flame Retardant grade With halogens | 6 g/10' | - | 2900 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® HK 20 TCH0 | 20% mineral filled polypropylene. Heast stabilized. | 6 g/10' | - | 2300 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 TFH0 | 20% mineral filled polypropylene. Heat stabilized. | 13 g/10' | - | 2300 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 TFHH | 20% talc filled polypropylene. Heat stabilized. Detergent Resistant. | 5 g/10' | - | 2200 Mpa | - | 3,9 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 TP F HS | 20% talc filled copolymer polypropylene. | 12 g/10' | - | 2200 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isofil® HK 25 6VH | 25% talc-calcium carbonate filled polypropylene. | 16 g/10' | - | 2400 Mpa | - | 5 KJ/m2 | - | Classe HB YC | |
Isofil® HK 25 GVH | 25% talc filled copolymer polypropylene. | 16 g/10' | - | 2200 Mpa | - | 5,1 KJ/m2 | - | Classe HB YC | |
Isofil® HK 25 GVH1 | 25% talc copolymer polypropylene. Heat stabilized. | 17 g/10' | - | 2000 Mpa | - | 12,9 KJ/m2 | - | Classe HB YC | |
Isofil® HK 25 TVH0 | 25% talc filled copolymer polypropylene. | 23 g/10' | - | 1800 Mpa | - | 7 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TFH2 | 30% talc filled polypropylene. | 14 g/10' | - | 34600 Mpa | - | 3,8 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TSH1 | 30% talc filled polypropylene homopolymer. Heat stabilized. | 3 g/10' | - | 3500 Mpa | - | 5 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TTH0 | 30% talc polypropylene. | 4 g/10' | - | 3300 Mpa | - | 3,1 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TTH1 | 30% talc filled polypropylene. UV stabilized. Heat stabilized. | 3 g/10' | - | 3400 Mpa | - | 2,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TVH0 | 30% talc filled homopolymer polypropylene. | 20 g/10' | - | 3400 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TVH2 | 30% talc filled polypropylene. | 16 g/10' | - | 3200 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TXH0 | 30% talc filled polypropylene. Heat stabilized. | 8 g/10' | - | 3300 Mpa | - | 2,7 KJ/m2 | - | Classe HB YC | |
Isofil® HK 35 GVH0 | 35% talc filled copolymer polypropylene. | 21 g/10' | - | 3100 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 2FH0 | 40% calcium carbonate filled polypropylene. Heat stabilized. | 13 g/10' | - | 2500 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 5FH0 | 40% calcium carbonate polypropylene. | 13 g/10' | - | 2500 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 TTH0 | 40% talc filled homopolymer polypropylene. Heat stabilized. | 4 g/10' | - | 3800 Mpa | - | 2,4 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 TVH0 | 40% talc filled copolymer polypropylene. | 18 g/10' | - | 4000 Mpa | - | 3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 50 2FH0 | 50% calcium carbonate filled polypropylene. | 20 g/10' | - | 2800 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® HK 50 C2 V | 50% calcium carbonate homopolymer polypropylene. Heat stabilized. | 18 g/10' | - | 3100 Mpa | - | 2,5 KJ/m2 | - | Classe HB YC | |
Isofil® HZ 9101D | 40% talc filled homopolymer polypropylene. Good flowability. | 23 g/10' | - | 4100 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® K 0 T xxx HB | Copolymer polypropylene. | 17 g/10' | - | 1200 Mpa | - | 7,9 KJ/m2 | - | Classe HB YC | |
Isofil® K 10 T 46.400 AFU | 10% talc filled copolymer polypropylene. Scratch resistant. UV stabilized. | 22 g/10' | - | 1300 Mpa | - | 40 KJ/m2 | - | Classe HB | |
Isofil® K 10 T 53.180U | 13% talc filled copolymer polypropylene. UV stabilized. Scratch Resistant. | 15 g/10' | - | 1650 Mpa | - | 18 KJ/m2 | - | Classe HB | |
Isofil® K 20 T 48.450 AFU | 20% talc filled copolymer polypropylene. Impact modified and scratch resistant. UV stabilized. | 19 g/10' | - | 1700 Mpa | - | 45 KJ/m2 | - | Classe HB | |
Isofil® K 20 T 50.400LCE SR AF | 17% talc filled copolymer polypropylene. Low CLTE and scratch resistant. UV stabilized. | 32 g/10' | - | 1450 Mpa | - | 40 KJ/m2 | - | Classe HB | |
Isofil® K 20 T xxx HB | 20% talc filled copolymer polypropylene. | 16 g/10' | - | 2300 Mpa | - | 6,5 KJ/m2 | - | Classe HB YC | |
Isofil® K 20 TP X | PP copo 20% talc | 10 g/10' | - | 2000 MPa | - | 7 Kj/m2 | - | Classe HB | |
Isofil® K 30 T 50.200LCE SR AF | 30% talc filled copolymer polypropylene. High impact. Scratch resistant. High fluidity. UV stabilized. | 33 g/10' | - | 1700 Mpa | - | 20 KJ/m2 | - | Classe HB | |
Isofil® K 30 T 60.90L | 30% talc filled copolymer polypropylene. UV stabilized. | 16 g/10' | - | 2300 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isofil® K 40 T | 40% talc filled polypropylene. | 7 g/10' | - | 4200 Mpa | - | 2,6 KJ/m2 | - | Classe HB | |
Isofil® K 40 T xxx HB | 40% talc filled copolymer polypropylene. Heat stabilized. | 8 g/10' | - | 3800 Mpa | - | 2,6 KJ/m2 | - | Classe HB YC | |
Isofil® K 40 TP V | PP copo 40% talc | 20 g/10' | - | 3400 MPa | - | 4,2 Kj/m2 | - | Classe HB | |
Isofil® KGF 4002U | 21,5% talc filled copolymer polypropylene. UV stabilized. | 12 g/10' | - | 2000 Mpa | - | 4 KJ/m2 | - | Classe HB | |
Isofil® KPZ 4001D | 20% talc filled copolymer polypropylene. Heat stabilized. | 20 g/10' | - | 2400 Mpa | - | 4,7 KJ/m2 | - | Classe HB YC | |
Isofil® MC 4214Y | 20% talc filled copolymer polypropylene. UV stabilized. Scratch Resistant. | 8 g/10' | - | 2300 Mpa | - | 7 KJ/m2 | - | Classe HB | |
Isofil® MF 3604Y | 16% talc filled polypropylene. Impact resistance grade. UV stabilized. Scratch Resistant. | 14 g/10' | - | 1500 Mpa | - | 30 KJ/m2 | - | Classe HB | |
Isofil® MF 4124S | 20% talc filled polypropylene compound. It exhibits high stiffness and low emission properties. Scratch Resistant. | 15 g/10' | - | 2700 Mpa | - | 4 KJ/m2 | - | Classe HB | |
Isofil® MV 4509Y | 20% talc filled polypropylene copolymer. Impact modified. UV stabilized. Scratch Resistant. | 26 g/10' | - | 1900 Mpa | - | 30 KJ/m2 | - | Classe HB | |
Isofil® MY 2205Y | 10% talc filled copolymer polypropylene. Low emission grade. Scratch Resistant. | 25 g/10' | - | 1600 Mpa | - | 18 KJ/m2 | - | Classe HB | |
Isofil® MZ 2102H | 10% talc filled homopolymer polypropylene. Low emission grade. | 25 g/10' | - | 2350 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® MZ 3506Y | 17% talc filled copolymer polypropylene. Good flowability. Low emission. UV stabilized. Heat stabilized. Scratch Resistant. | 22 g/10' | - | 2000 Mpa | - | 25 KJ/m2 | - | Classe HB | |
Isofil® PF 4102H | 20% Talc filled polypropylene homopolymer. Low emission. Compliant to VW44045-PP6 and WSS-M4D729-B1. Heat stabilized. | 12 g/10' | - | 2800 Mpa | - | 3 KJ/m2 | - | Classe HB | |
Isofil® PZ 8103H | 40% talc filled polypropylene homopolymer. Heat stabilized. | 20 g/10' | - | 4300 Mpa | - | 3 KJ/m2 | - | Classe HB | |
Isofil® RF 3403Y | 15% talc filled polypropylene copolymer. Impact modified. High fluidity. Low CLTE. UV stabilized. Scratch Resistant. | 15 g/10' | - | 1700 Mpa | - | 25 KJ/m2 | - | Classe HB | |
Isofil® RV 4603S | 20% talc filled impact modified polypropylene. Compliant to TL 52388-F. UV stabilized. Scratch Resistant. | 18 g/10' | - | 2000 Mpa | - | 35 KJ/m2 | - | Classe HB | |
Isofil® SF 4303U | 20% talc filled copolymer polypropylene with good stiffness and impact resistance. UV stabilized. | 15 g/10' | - | 1800 Mpa | - | 15 KJ/m2 | - | Classe HB | |
Isofil® SF 4501Y | 20% talc filled copolymer polypropylene. Impact modified grade. UV stabilized. Scratch Resistant. | 14 g/10' | - | 1900 Mpa | - | 20 KJ/m2 | - | Classe HB | |
Isofil® SV 4118X | 20% talc filled homopolymer polypropylene. Compliant to TL 52658-WD01. UV stabilized. Heat stabilized. | 16 g/10' | - | 2800 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® SV 4205Y | 20% talc filled polypropylene copolymer. Good flowability and stiffness. UV stabilized. Scratch Resistant. | 16 g/10' | - | 2300 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isofil® SW 4909U | 20% talc filled copolymer polypropylene. Impact modified grade with high flowability. UV stabilized. | 40 g/10' | - | 1500 Mpa | - | 40 KJ/m2 | - | Classe HB |
Isoglass®
Polipropilene compound rinforzato con fibre di vetro, legate chimicamente o meccanicamente, con elevate proprietà termiche, di resistenza all’impatto e di rigidità, in accordo con gli standard delle industrie automobilistiche e dell’elettrodomestico. Prodotti disponibili nelle colorazioni e nelle versioni autoestinguenti indicate per i relativi settori, con importanti certificazioni per alogenati e esente alogeni.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Isoglass® 4F 4030U | 22% chemically coupled glass fiber and mineral filled reinforced polypropylene copolymer. Good stiffness and impact strenght balance combined with high flowability. UV stabilized. | 14 g/10' | - | 3200 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® EV 3007U | 15% chemically coupled glass fiber reinforced polypropylene copolymer. High flowability grade and good aesthetical appearance. UV stabilized. | 18 g/10' | - | 2600 Mpa | - | 12 KJ/m2 | - | Classe HB | |
Isoglass® H 20 CGF X | 20% glass fiber reinforced homopolymer polypropylene. | 8 g/10' | - | 3800 MPa | - | 8 Kj/m2 | - | Classe HB | |
Isoglass® H 20 CGF X HS | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to VW 44045-PP9. Heat stabilized. | 8 g/10' | - | 4000 Mpa | - | 7 KJ/m2 | - | Classe HB | |
Isoglass® H 20 FVL X | 20% glass fiber polypropylene. Heat stabilized. | 8 g/10' | - | 3900 Mpa | - | 7,4 KJ/m2 | - | Classe HB YC | |
Isoglass® H 25 CGF C UV | 25% chemically coupled glass fibre reinforced Polypropylene. Antistatic.UV stabilized. | 6 g/10' | - | 5400 Mpa | - | 11 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF 140.80 | 30% glass fiber reinforced homopolymer polypropylene. Compliant to MS-55246 PP140.80. Heat stabilized. | 18 g/10' | - | 5700 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF C | 30% chemically coupled glass fiber reinforced polypropylene. Heat stabilized. | 5 g/10' | - | 6000 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF C UV | 30% chemically coupled glass fiber reinforced polypropylene. Low odor and emission. Compliant to VW44045-PP10 and VW50180. UV stabilized. Heat stabilized. | 5 g/10' | - | 5800 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF F UV | 30% glass fiber reinforced homopolymer polypropylene. UV stabilized. | 13 g/10' | - | 5000 Mpa | - | 8 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF S HS | 30% glass fiber reinforced homopolymer polypropylene. Heat stabilized. | 5 kg/10' | - | 6000 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF X HS | 30% chemically coupled glass fiber reinforced polypropylene. Heat stabilized. | 8 g/10' | - | 6000 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® H 30 FVL C | PP homo 30% glass fiber. Heat stabilized. | 6 g/10' | - | 5800 MPa | - | 11,5 Kj/m2 | - | Classe HB YC | |
Isoglass® H 30 FVL V | 30% glass fiber filled homopolymer polypropylene. | 20 g/10' | - | 5700 Mpa | - | 10 KJ/m2 | - | Classe HB YC | |
Isoglass® H 30 GFT3 C HS | 30% glass fiber and talc filled polypropylene. Compliant to MS-55246 PP130.50. Heat stabilized. | 8 g/10' | - | 4500 Mpa | - | 7 KJ/m2 | - | Classe HB | |
Isoglass® H 40 CGF C | 40% glass fiber reinforced homopolymer polypropylene. | 7 g/10' | - | 7600 MPa | - | 9 Kj/m2 | - | Classe HB | |
Isoglass® H3V 6009D | 30% talc filled and glass fiber reinforced polypropylene homopolymer. Heat stabilized. Detergent resistant. | 17 g/10' | - | 4700 Mpa | - | 5 KJ/m2 | - | Classe HB YC | |
Isoglass® HGV 6002D | 30% glass fiber homopolymer polypropylene. Heat stabilized. Detergent Resistant. | 17 g/10' | - | 5600 Mpa | - | 9,1 KJ/m2 | - | Classe HB YC | |
Isoglass® HGV 6003X | 30% chemically coupled glass fiber reinforced polypropylene. High flowability. UV stabilized. Chemical Resistant. | 20 g/10' | - | 5500 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® K 20 CGF X | 20% glass fiber reinforced copolymer polypropylene. | 10 g/10' | - | 3400 Mpa | - | 13 KJ/m2 | - | Classe HB | |
Isoglass® K 30 CGF X | 30% glass fiber reinforced copolymer polypropylene. | 8 g/10' | - | 4000 Mpa | - | 16 KJ/m2 | - | Classe HB | |
Isoglass® K 40 CGF C | 40% glass fiber reinforced copolymer polypropylene. | 4 g/10' | - | 6200 MPa | - | 15 Kj/m2 | - | Classe HB | |
Isoglass® SC 6029X | 30% chemically coupled glass fiber reinforced copolymer polypropylene. UV stabilized. Heat stabilized. | 5 g/10' | - | 4500 Mpa | - | 22 KJ/m2 | - | Classe HB | |
Isoglass® ST 8020N | 40% chemically coupled glass fiber reinforced polypropylene homopolymer. UV stabilized. Heat stabilized. | 4 g/10' | - | 8000 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® SX 4010H | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to Renault-Nissan AS8. Heat stabilized. | 10 g/10' | - | 4000 Mpa | - | 8 KJ/m2 | - | Classe HB | |
Isoglass® SX 4015X | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to VW 44045. UV stabilized. Heat stabilized. | 8 g/10' | - | 3800 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isoglass® SX 8022H | 40% chemically coupled glass fiber reinforced polypropylene homopolymer. Heat stabilized. | 10 g/10' | - | 7700 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® XX 6014D | 30% chemically coupled glass fiber reinforced polypropylene, high stiffness. Heat stabilized. | 8 g/10' | - | 7000 Mpa | - | 9 KJ/m2 | - | Classe HB |
Isoglass® XT
Polipropilene compound rinforzato con fibre di vetro, legate chimicamente o meccanicamente, con elevate proprietà termiche, di resistenza all’impatto e di rigidità, in accordo con gli standard delle industrie automobilistiche e dell’elettrodomestico. Prodotti disponibili nelle colorazioni e nelle versioni autoestinguenti indicate per i relativi settori, con importanti certificazioni per alogenati e esente alogeni.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Isoglass® XT 1003H | 50% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness grade. Heat stabilized. | 3,5 g/10' | - | 13000 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® XT 4001D | 20% chemically coupled glass fiber reinforced polypropylene. | 7 g/10' | - | 4000 Mpa | - | 7 KJ/m2 | - | Classe HB YC | |
Isoglass® XT 4007U | 20% chemically coupled high performance reinforced polypropylene homopolymer. High stiffness and low emission. Compliant to DBL 5430. UV stabilized. | 7 g/10' | - | 6100 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® XT 6001D | 30% chemically coupled high performance glass fiber reinforced polypropylene compound. | 5 g/10' | - | 6800 Mpa | - | 11 KJ/m2 | - | Classe HB YC | |
Isoglass® XT 6001H | 30% chemically coupled high performance glass fiber reinforced polypropylene. Heat stabilized. | 3,5 g/10' | - | 6500 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® XT 6010H | 30% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness and low emission. | 6 g/10' | - | 8400 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® XT 7001H | 35% chemically coupled glass fiber reinforced polypropylene homopolymer. Low flowability grade. Heat stabilized. | 3 g/10' | - | 8000 Mpa | - | 12 KJ/m2 | - | Classe HB | |
Isoglass® XT 8008H | 40% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness and low emission. | 5 g/10' | - | 10000 Mpa | - | 10 KJ/m2 | - | Classe HB |
Isoglass® LFT
Polipropilene compound rinforzato con fibre di vetro lunghe, ottenuto per pultrusione, che presenta elevate prestazioni termico-meccaniche. Particolarmente indicato in applicazioni strutturali, in cui è possibile sfruttare l’orientazione delle fibre lunghe per incrementare la stabilità dimensionale e la rigidezza del manufatto. Disponibili prodotti con contenuti di fibra in diverse percentuali, anche elevate.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Isoglass® LFT 1001H | PP homo 50% long glass fiber, heat stabilized. | / | - | 10500 MPa | - | 29 Kj/m2 | - | Classe HB | |
Isoglass® LFT LFT 0603H | 30% chemically coupled long glass fiber reinforced polypropylene compound with very high mechanical properties and heat stabilized. | / | - | 6300 Mpa | - | 21 Kj/m2 | - | Classe HB |
Green Isofil®
Polipropilene compound additivato con cariche minerali contenente percentuali di materiale riciclato post-industriale o post-consumo. I prodotti rispettano gli standard recentemente introdotti dai settori auto ed elettrodomestico.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Green Isofil® HK 40 C F | PP copo 40% calcium carbonate, heat stabilized, detergent resistant. | 20 g/10' | - | 1900 MPa | - | 3,3 Kj/m2 | - | Classe HB | |
Green Isofil® K 30 T T HS | 30% talc filled polypropylene copolymer. Industrial quality. Heat stabilized. | 3 g/10' | - | 2200 MPa | - | 6 Kj/m2 | - | Classe HB |
Green Isoglass®
Polipropilene compound rinforzato con fibre di vetro contenente percentuali di materiale riciclato post-industriale o post-consumo. I prodotti rispettano gli standard recentemente introdotti dai settori auto ed elettrodomestico.Nome | Compound | MFR ISO 1133 | MFI (g/10’) ASTM D1238 | MEF ISO 178 | MFI (g/10’) ASTM D1238 | Izod Notched ISO 180/1A | Izod Notched (J/m²) ASTM D256 | Infiammabilità UL94 | |
---|---|---|---|---|---|---|---|---|---|
Green Isoglass® H 30 CGF C HS | 30% chemically coupled glass fiber reinforced polypropylene with 30% circular polymer source. Heat stabilized. | 6 g/10' | - | 4900 MPa | - | 9 Kj/m2 | - | Classe HB | |
Green Isoglass® H 40 CGF X HS | 40% glass fiber reinforced polypropylene. Industrial quality. Heat stabilized. | 10 g/10' | - | 6000 MPa | - | 9 Kj/m2 | - | Classe HB |